Testing water resistance of coatings using water fog apparatus
Can be used to test the water resistance of coatings by exposing coated specimens to water fog at an elevated temperature, using apparatus similar to that used for salt spray testing to ASTM B117.
Test specimens are placed in an enclosed chamber that meets the apparatus requirements of ASTM B117. Here they are exposed to a continuous indirect spray water, which falls-out on to the specimens at a rate of 1.5 to 3.0ml/80cm²/hour, in a chamber temperature of +38C. Este clima se mantiene en condiciones de estado estable constante. La duración de la prueba es variable.
Para obtener más información sobre las normas ASTM, visite; www.astm.com
Prueba de Humedad (General Motors)
Se puede utilizar para probar muestras recubiertas exponiéndolas a la niebla del agua a una temperatura elevada, utilizando aparatos similares a los utilizados para las pruebas de pulverización de sal a ASTM B117.
Test specimens are placed in an enclosed chamber that meets the apparatus requirements of ASTM B117. Aquí se exponen a un agua continua de pulverización indirecta, que cae sobre los especímenes a una velocidad de 1.0 a 2.0ml/80cm2/hora, en una temperatura de cámara de +38C y una humedad de 100% HR. Este clima se mantiene en condiciones de estado estable constante. La duración de la prueba es variable.
Para más información sobre las normas de General Motors visite; www.global.ihs.com