UNI EN ISO 6988
Kesternich 测试模拟酸雨或工业化学品暴露,以评估涂层、基材或部件本身的相对耐腐蚀性。 零件或面板放置在专门设计的腔室中,并暴露于SO2和湿度下,然后进行耐腐蚀性评估。 以下标准用于此类测试。
UNI EN ISO 6988测试标准用于金属涂层和其他非有机涂层。 该标准规定了评估材料或产品对含有冷凝水分和二氧化硫的大气的耐腐蚀性的方法。 该方法被发现适用于评估金属涂层和其他非有机涂层。