ISO 6270-2 (AHT)

在冷凝水气氛中暴露试样的程序。

ISO 6270-2 (AHT)

该测试标准取代了DIN 50 017*,并且类似于DIN 50 017 *。

测试“AHT”(湿度和空气温度交替的冷凝气氛) – 需要改变40°C至18-28°C的温度条件,在此期间湿度从c.100%RH的冷凝水平变化到环境湿度水平。

* 上述 6270-2 测试方法与 DIN 50 017 测试方法之间的相关性为:
6270-2 方法“AHT”相当于 DIN 50 017 方法“KFW”。