Corrosion Testing Standards

The test standard summaries are for general guidance only. Though believed to be accurate at the time of writing, this may change over time. So this information should not be used as a substitute for referring to a complete test standard, at an appropriate revision level.

Note: the terms salt spray, salt mist and salt fog are all in wide spread use within corrosion test standards. In this context they can be considered to be equivalent and interchangeable terms.

DIN 50 021-CASS

DIN 50 021-CASS  Copper Chloride Acetic Acid Salt Spray Test

Can be used to test the relative resistance to corrosion of coatings, when exposed to a copper accelerated acetic acid salt spray climate at an elevated temperature.

Test specimens are placed in an enclosed chamber and exposed to a continuous indirect spray of acidified (pH 3.1to 3.3) salt water solution, which falls-out on to the specimens at a rate of 1.0 to 2.0ml/80cm²/hour, in a chamber temperature of +50C. This climate is maintained under constant steady state conditions. The test duration is variable.

For further information on DIN standards and DIN 50 021-CASS visit; www.din.de