DIN 50 017-KFW

冷凝水测试气候

DIN 50 017-KFW

将试样置于封闭的腔室中,并暴露于由以下两部分重复循环组成的气候变化中。 在加热的饱和空气和水蒸气混合物中暴露8小时,温度为+ 40C,相对湿度为100%RH。 随后暴露在室温(根据 DIN 50 014 为 +18 至 +28C)和相对湿度小于 100%RH 的条件下 16 小时。 重复周期的次数,因此测试持续时间是可变的。