DEF STAN 1053 方法 24

DEF STAN 1053方法24可用于测试当暴露于环境温度下的盐雾气候时涂漆样品的相对耐腐蚀性。

将试样置于封闭的腔室中,并暴露于合成海水溶液的连续间接喷雾中,该合成海水溶液以每小时消耗1.0至1.5升盐溶液的速度落在试样上,在+ 20C的腔室温度下。 这种气候在恒定的稳态条件下保持。 DEF STAN 1053方法24的测试持续时间是可变的。

该测试也称为“冷”盐雾测试。