The test standard summaries are for general guidance only. Though believed to be accurate at the time of writing, this may change over time. So this information should not be used as a substitute for referring to a complete test standard, at an appropriate revision level.
Note: the terms salt spray, salt mist and salt fog are all in wide spread use within corrosion test standards. In this context they can be considered to be equivalent and interchangeable terms.
DEF STAN 00-35 Pt3 CN2
盐(腐蚀性)气氛
DEF STAN 00-35 Pt3 CN2
该国防标准测试的目的是确定材料对含盐大气的抵抗力。 它涵盖了两种不同的测试方法,在“盐雾测试”和“盐腐蚀测试”中称为” 详情如下:
盐雾测试
该测试基于测试标准BS EN 60068-2-11。 有关BS EN 60068-2-11的详细信息,请参阅本文档的其他地方。
盐腐蚀试验