Corrosion Testing Standards

The test standard summaries are for general guidance only. Though believed to be accurate at the time of writing, this may change over time. So this information should not be used as a substitute for referring to a complete test standard, at an appropriate revision level.

Note: the terms salt spray, salt mist and salt fog are all in wide spread use within corrosion test standards. In this context they can be considered to be equivalent and interchangeable terms.

BS 3900 第 F2 部分

冷凝条件下耐湿性的测定

可用于测试涂层试样在温度循环气候条件下对冷凝条件的抵抗力。

将试样放置在封闭的腔室中,其中产生由空气和水蒸气的加热饱和混合物组成的气候,温度在+ 42C和+ 48C之间连续循环,相对湿度恒定为100%RH。 从42C到48C和回到42C的每个循环所需的时间应为60分钟,加热和冷却时间大致相等。 重复周期的次数,因此测试持续时间是可变的。

有关英国标准的更多信息,请访问; www.bsigroup.com