ASTM B287

醋酸盐雾(雾)测试

可用于测试在高温下暴露于乙酸盐雾气候时无机和有机涂层黑色金属和有色金属的相对耐腐蚀性。

将试样置于封闭的腔室中,并暴露于酸化(pH 3.1至3.3)盐水溶液的连续间接喷雾中,该溶液以0.75至2.0ml / 80cm² /小时的速率在+35C的腔室中落到试样上。 这种气候在恒定的稳态条件下保持。 测试持续时间是可变的。

此测试也称为 ASS 测试。

有关ASTM标准的更多信息,请访问; www.astm.com

注意;ASTM B287 已被 ASTM G85 附录 A1 取代