Corrosion Testing Standards

The test standard summaries are for general guidance only. Though believed to be accurate at the time of writing, this may change over time. So this information should not be used as a substitute for referring to a complete test standard, at an appropriate revision level.

Note: the terms salt spray, salt mist and salt fog are all in wide spread use within corrosion test standards. In this context they can be considered to be equivalent and interchangeable terms.

50180 方法 A1

盐雾试验(菲亚特)

50180 方法 A1

可用于测试金属基材上无机和有机涂层在高温下暴露于盐雾气候下的相对耐腐蚀性。

将试样置于封闭的腔室中,并暴露于连续间接喷洒中性(pH 6.5至7.2)盐水溶液,该溶液以1.0至2.0ml / 80cm² /小时的速率在+35C的腔室温度下落到试样上。 这种气候在恒定的稳态条件下保持。 测试持续时间是可变的。

这是菲亚特测试标准。