福特 FLTM BI 123-03

部件腐蚀测试

该测试程序用于评估应用于组件的涂层的腐蚀性能。 它旨在模拟亚利桑那州试验场(APG)车辆加速腐蚀试验(CETP 00.00-R-311)的腐蚀条件。 该测试需要一个自动循环腐蚀试验箱,具有强制空气循环,温度控制在+/- 2°C至65°C,相对湿度控制为+/- 2%至90%。