菲亚特 50493

有机涂层在表皮腐蚀下对气泡传播的抵抗力的测定

菲亚特 50493

也称为 SCAB 室内腐蚀试验

1 小时湿度测试,55°C / 95% RH

然后在55°C / 55-60%RH下进行40分钟的温控空气干燥

空气干燥阶段需要在20分钟内到达