The test standard summaries are for general guidance only. Though believed to be accurate at the time of writing, this may change over time. So this information should not be used as a substitute for referring to a complete test standard, at an appropriate revision level.
Note: the terms salt spray, salt mist and salt fog are all in wide spread use within corrosion test standards. In this context they can be considered to be equivalent and interchangeable terms.
Fiat 50493
Determination of the resistance of organic coatings to the propagation of bubble under skin corrosion
Fiat 50493
also known as SCAB indoor corrosion test
1 hour humidity test at 55°C / 95% RH
Followed by 40 minutes of temperature controlled air drying @ 55°C / 55-60% RH
The air drying stage needs to be reached within 20 minutes