Atmosfär Premium Specifications

AtmosfärPremium Specifications for range of Corrosion Equipment

Wetting mode  Temperature range  Adjustable from ambient to +70°C/+158°F
  Humidity range  Fixed at 95% – 100% RH
Oscillating Salt spray mode  Temperature range  Adjustable from ambient to +60°C/+140°F
  Salt spray fall-out rates  Adjustable from 5 to 10 Ltrs/m² per hour
Conventional Salt spray mode  Temperature range  Adjustable from ambient to +60°C/+140°F
  Salt spray fall-out rates  Adjustable from 0.5 to 5.5 ml per 80 cm² per hour
Drying mode Temperature range  Adjustable from ambient to +80°C/+176°F
  Humidity range  Uncontrolled
Climatic mode Temperature/humidity range  See graph below

Performance Graph

Graph showing range of temperature/humidity control for AtmosfärPremium Corrosion Testing Equipment.
  • Light Blue shaded area is the standard AtmosfärPremiumLite chamber control
  • Royal Blue shaded area is the additional control of the AtmosfärPremium sub zero chambers which includes the ACC29 Air temperature control unit.
  • Dark Blue is the maximum temperature and humidity achieved by any AtmosfärPremium chamber.

Contact us for further information or assistance.

Atmosfär test chambers AT1300iPLite AT1300iP AT1300iP AT2600IPLite AT2600iP AT2600iP
Minimum Controlled Temperature  +20°/ +68°F -20°C/-4°F -40°C/ -40°F +20°/ +68°F -20°C/-4°F -40°C/ -40°F
Chamber Capacity 1300 Ltrs/45.9 cu.ft 1300 Ltrs/45.9 cu.ft 1300 Ltrs/45.9 cu.ft 2600 Ltrs/91.8 cu.ft 2600 Ltrs/91.8 cu.ft 2600 Ltrs/91.8 cu.ft
Chamber weight (estimated, without optional accessories) 340 kg 340 kg 340 kg 440 kg 440 kg 440 kg
Mounting Format Floor standing Floor standing Floor standing Floor standing Floor standing Floor standing
Loading threshold 800mm/31.5″ 800mm/31.5″ 800mm/31.5″ 800mm/31.5″ 800mm/31.5″ 800mm/31.5″
Chamber external dims, max W 2025mm/80.0″ 2025mm/80.0″ 2025mm/80.0″ 2885mm/113.6″ 2885mm/113.6″ 2885mm/113.6″
D 1316mm/51.8″ 1316mm/51.8″ 1316mm/51.8″ 1250mm/49″ 1250mm/49″ 1250mm/49″
H 1965mm/77.4″ 1965mm/77.4″ 1965mm/77.4″ 1946mm/77″ 1946mm/77″ 1946mm/77″
Chamber internal dims, max W 1300mm/51.2″ 1300mm/51.2″ 1300mm/51.2″ 2160mm/85.0″ 2160mm/85.0″ 2160mm/85.0″
D 980mm/38.5″ 980mm/38.5″ 980mm/38.5″ 980mm/38.5″ 980mm/38.5″ 980mm/38.5″
H 1500mm/59.0″ 1500mm/59.0″ 1500mm/59.0″ 1500mm/59.0″ 1500mm/59.0″ 1500mm/59.0″
Refrigeration unit Separate unit, one supplied to be located on the left hand side of the AtmosfärPremium chamber W 626mm/25″ 1125mm/44.3″ 1125mm/44.3″ 626mm/25″ 1125mm/44.3″ 1125mm/44.3″
D 1522mm/60″ 1354mm/53.3″ 1354mm/53.3″” 1522mm/60″ 1354mm/53.3″ 1354mm/53.3″
H 1080mm/42″ 1624mm/63.9″ 1624mm/63.9″ 1080mm/42″ 1624mm/63.9″ 1624mm/63.9″
Salt solution reservoir 90 Ltrs/23 US gal

Separate unit, one supplied to deliver salt water to the conventional salt spray atomizer

W 540mm/21″ Dia 540mm/21″ Dia 540mm/21″ Dia 540mm/21″ Dia 540mm/21″ Dia 540mm/21″ Dia
D 540mm/21″ Dia 540mm/21″ Dia 540mm/21″ Dia 540mm/21″ Dia 540mm/21″ Dia 540mm/21″ Dia
H 635mm/25″ 635mm/25″ 635mm/25″ 635mm/25″ 635mm/25″ 635mm/25″
Salt solution reservoir 160 Ltrs/42.2 US gal 

Separate unit, one supplied to deliver salt water to the spray bar

W 840mm/34.0″ 840mm/34.0″ 840mm/34.0″ 840mm/34.0″ 840mm/34.0″ 840mm/34.0″
D 500mm/19.7″ 500mm/19.7″ 500mm/19.7″ 500mm/19.7″ 500mm/19.7″ 500mm/19.7″
H 790mm/31.1″ 790mm/31.1″ 790mm/31.1″ 790mm/31.1″ 790mm/31.1″ 790mm/31.1″
Chamber construction Glass reinforced plastic, Polypropylene & ABS parts
Color 9 standard colors to choose from free of charge
Electricity supply Voltage (VAC) and frequency (Hz) dependant on country/region of installation.
Water Deionized/distilled for topping up air saturator and making salt solution. The continuous water supply must be pressurized 4.0 – 5.0 bar (58-72 psi). If air saturator is intended to be topped up manually option ACC66 must be ordered.
Air Clean dry and oil free compressed air, 4.0 to 6.0 bar (58-87psi) with 440 Ltrs (15.5cu.ft) per minute flow. Two separate supplies are required, one for the chamber and one for the separate refrigeration unit.
Exhaust 3m (10ft) exhaust pipe is required which should be terminated outside building (see accessory ACC58
Drain 3m (10ft) drain pipe is required which should be terminated into floor level drain (see accessory ACC58)
Operating environment conditions Indoors, with ambient maintained at +18 to +23°C (+64 to 73°F), 85% max RH (non-condensing).