Kesternich – Key Features
Ascott Kesternich Chamber
KH300 – Fully Automatic, SO2 Gas Dosing Test Chamber
![Ascott Kesternich Chamber](https://www.ascott-analytical.com/wp-content/uploads/2021/11/KH300.jpg)
Kesternich testing simulates acid rain or industrial chemical exposure to evaluate the relative corrosion resistance of the coating, substrate, or part itself. Parts or panels are placed inside a specially designed chamber and are exposed to SO2 and condensation humidity before being evaluated for resistance to corrosion.
A specific volume of SO2 gas, usually 0.2L, 1L or 2L is introduced into the test chamber, the chamber temperature is increased to a predetermined level and the relative humidity is maintained at condensation levels. After a set period, the chamber is vented and the temperature is allowed to decrease to ambient conditions.
Ascott’s Kesternich chamber does not require any human intervention whilst running the tests, its fully automatic design is controlled by a state of the art control system. The Kesternich chamber is designed to meet various gas dosing test standards as listed below and can also be used as a condensation humidity chamber.
Features of the Kesternich Chamber:
- SO2/Humidity mode
- Condensation Humidity mode
- Air Flushing mode
- Fully automated electronic gas dosing system
- Hermetically sealed chamber with Automatic air purge function with canopy interlock
- User friendly control system with Pneumatic canopy control
- Automatic drain and exhaust system
- Digital precision temperature control
- Temperature graphical display
- Interior viewing window with illumination
- Ethernet communication port
Also available as a table-top version
Click here to watch a video on the overview of our Ascott Kesternich Chambers
![](https://www.ascott-analytical.com/wp-content/uploads/2021/11/ASCOTT-23-1024x683.jpg)
![](https://www.ascott-analytical.com/wp-content/uploads/2021/11/ASCOTT-24-1024x683.jpg)
Fully complies with the following standards:
ASTM D2247, ISO 11503, NFT 30-077, NFT 30-055, ASTM G87, BS3900/F9, ISO 6270-2 CH, EN ISO 6988, SFW 2,0,S, ISO EN 1096 B, ISO 22479, DIN 50017 KK & KTW, ISO 3231, DIN 50018, VDA 621-421, ISO EN 1096 C
Technical Specification
- Volume: 300L
- Internal Dimensions: 730 x 496 x 851 reducing to 534mm (w x d x h) angled interior roof to avoid droplets
- External Dimensions: 1200 x 760 x 2000mm (w x d x h)
- Temperature Range: Ambient to +50ºC/122ºF
- Temperature Stability: +/- 0.75ºC
- Power Supply: 220-240V, Single Phase 50Hz
For further information contact us on the form below, alternatively, to speak with one of our sales representatives call us on +44 (0) 1827 318040