Corrosion Testing Standards

The test standard summaries are for general guidance only. Though believed to be accurate at the time of writing, this may change over time. So this information should not be used as a substitute for referring to a complete test standard, at an appropriate revision level.

Note: the terms salt spray, salt mist and salt fog are all in wide spread use within corrosion test standards. In this context they can be considered to be equivalent and interchangeable terms.

ASTM D1748

湿度柜中金属防腐剂防锈的测试方法

本标准规定了在高湿度条件下评估金属防腐剂防锈性能的测试方法。 钢板准备到规定的表面光洁度,浸入测试油中,让其排水。 然后将它们悬浮在特殊设计的湿度室中(必须符合军事规范JAN-H-792的要求),在那里它们暴露在48.9C(120F)的温度和高(未指定)相对湿度下。 这种气候在恒定的稳态条件下保持。 测试持续时间是可变的。

雅诗阁目前不制造符合此测试方法的腐蚀试验箱。

有关ASTM标准的更多信息,请访问; www.astm.com