The test standard summaries are for general guidance only. Though believed to be accurate at the time of writing, this may change over time. So this information should not be used as a substitute for referring to a complete test standard, at an appropriate revision level.
Note: the terms salt spray, salt mist and salt fog are all in wide spread use within corrosion test standards. In this context they can be considered to be equivalent and interchangeable terms.
标准偏差 5711,102
人工大气中的腐蚀测试 – 盐雾测试
该沃尔沃汽车测试标准与ISO 9227(人造大气中的盐雾腐蚀测试)相同。 单击此处 查看 ISO 9227 标准测试的详细信息。
有关沃尔沃标准的更多信息,请访问; volvogroup.com/suppliers