DIN 50 021-化学社会保险
氯化铜醋酸盐雾试验
可用于测试涂料的相对耐腐蚀性,当暴露在高温下的铜加速乙酸盐雾气候下时。
将试样置于封闭的腔室中,并暴露于酸化(pH 3.1至3.3)盐水溶液的连续间接喷雾中,该溶液以1.0至2.0ml / 80cm² /小时的速率在+50C的腔室温度下落到试样上。 这种气候在恒定的稳态条件下保持。 测试持续时间是可变的。