Corrosion Testing Standards

The test standard summaries are for general guidance only. Though believed to be accurate at the time of writing, this may change over time. So this information should not be used as a substitute for referring to a complete test standard, at an appropriate revision level.

Note: the terms salt spray, salt mist and salt fog are all in wide spread use within corrosion test standards. In this context they can be considered to be equivalent and interchangeable terms.

BS2011 Part2.1 Ka

基本环境测试程序,盐雾

可用于测试保护涂层在高温下暴露于盐雾(喷雾)气候时的相对耐腐蚀性。

将试样置于封闭的腔室中,并暴露于连续间接喷洒中性(pH 6.5至7.2)盐水溶液,该溶液以1.0至2.0ml / 80cm² /小时的速率在+35C的腔室温度下落到试样上。 这种气候在恒定的稳态条件下保持。 测试持续时间是可变的。

该测试也称为中性盐雾或NSS测试。

有关英国标准的更多信息,请访问; www.bsigroup.com