Corrosion Testing Standards

The test standard summaries are for general guidance only. Though believed to be accurate at the time of writing, this may change over time. So this information should not be used as a substitute for referring to a complete test standard, at an appropriate revision level.

Note: the terms salt spray, salt mist and salt fog are all in wide spread use within corrosion test standards. In this context they can be considered to be equivalent and interchangeable terms.

AA-0224 (AA-P 175)

验证表面涂层和粘合剂粘合的腐蚀行为。

AA-0224 (AA-P 175) 是一项为期 7 天的循环腐蚀测试 (CCT),包括以下步骤:

星期一:根据AA-0324开始循环24小时盐雾。
周二至周五:08:00至16:00,根据AA-0213标准,在40°C下冷凝水恒温。
从16.00到08.00小时在室温下再生(打开的腔室或通风室)
周六至周日:室温再生(打开的腔室或通风室)