Corrosion Testing Standards

The test standard summaries are for general guidance only. Though believed to be accurate at the time of writing, this may change over time. So this information should not be used as a substitute for referring to a complete test standard, at an appropriate revision level.

Note: the terms salt spray, salt mist and salt fog are all in wide spread use within corrosion test standards. In this context they can be considered to be equivalent and interchangeable terms.

TPJLR.52.252

Método de ensaio para resistência ao nevoeiro salgado (Jaguar)

TPJLR.52.252

Esta norma de teste automóvel Jaguar baseia-se na norma de teste ASTM B117. Consulte em outro lugar neste documento para mais detalhes sobre a ASTM B117.