Corrosion Testing Standards

The test standard summaries are for general guidance only. Though believed to be accurate at the time of writing, this may change over time. So this information should not be used as a substitute for referring to a complete test standard, at an appropriate revision level.

Note: the terms salt spray, salt mist and salt fog are all in wide spread use within corrosion test standards. In this context they can be considered to be equivalent and interchangeable terms.

DST 5711,102

Teste de corrosão em atmosferas artificiais – testes de spray de sal

Este padrão de teste automóvel volvo é o mesmo que ISO 9227 (Testes de corrosão de spray de sal em atmosferas artificiais). Clique aqui para ver detalhes do teste padrão ISO 9227.