Model reference

 

CC450xp

CC1000xp

CC2000xp

 
 
 
 
 

Chamber Capacity

 

450 Ltrs/
15.8 cu ft

1000 Ltrs/
35.3 cu ft

2000 Ltrs/
70.6 cu ft

 
 
 
 
 

Mounting Format

 

Floor standing

Floor standing

Floor standing

 
 
 
 
 

Loading threshold

 

800mm/31.5"

800mm/31.5"

800mm/31.5"

 
 
 
 
 

Chamber external dims, max

W  

1660mm/65.4"

2025mm/80.0"

2885mm/113.6"

D  

840mm/33.1"

1205mm/47.5"

1205mm/47.5"

H  

1510mm/59.5"

1720mm/67.5"

1720mm/67.5"

 
 
 
 
 

Chamber internal dims, max

W  

1010mm/39.5"

1350mm/51.0"

2160mm/85.0"

D  

640mm/25.0"

980mm/38.5"

980mm/38.5"

H  

1140mm/45.0"

1320mm/52.0"

1320mm/52.0"

 
 
 
 
 

Salt solution reservoir ext. dims.

W  

330mm/13.0"

330mm/13.0"

330mm/13.0"

D  

620mm/24.5"

620mm/24.5"

620mm/24.5"

H  

700mm/27.5"

700mm/27.5"

700mm/27.5"

 
 
 
 
 

Salt solution reservoir capacity for extra capacity, see optional accessory ACC02

 

100 Ltrs/
26 USgal

140 Ltrs/
37 USgal

140 Ltrs/
37 USgal

 
 
 
 
 

Removable slotted sample racks see also optional accessories
ACC17/ACC18)

 

6 racks each
with 28 angled slots

8 racks each with 46 angled slots

16 racks each with 46 angled slots

 
 
 
 
 

Chamber construction

 

Glass reinforced plastic, Polypropylene & PVC parts

 
 
 
 
 

Color

 

White & light gray with a striking turquoise canopy (alternative canopy colors available - see optional accessory ACC60)

 
 
 
 
 

Modes of operation

 

 

Condensation humidity mode

Temperature range

Adjustable from ambient to +50°C/+122°F

 

Humidity range

Fixed at 95% - 100% RH

 
 
 
 
 

Salt spray mode

Temperature range

Adjustable from ambient to +50°C/+122°F

 

Salt fog fall-out rate

Adjustable from 0.5 tp 3.0ml per 80cm² per hr

 
 
 
 
 

Air drying mode

Temperature range

Adjustable from ambient to +70°C/+158°F

 

Humidity range

Uncontrolled

 
 
 
 
 

Controlled humidity mode

Temperature range

Click to see graph

 

Humidity range

Click to see graph

 
 
 
 
 

Service utilities required

 

 

Electricity supply

 

3 phase, voltage (VAC) and frequency (Hz) dependant on country/region of installation

 
 
 
 
 

Water

 

Deionized/distilled for topping up air saturator and making salt solution. Air saturator requires a continuous water connection 0.5-6.0 bar (7.3-87 psi). If air saturator is topped up manually option ACC66 must be ordered

 
 
 
 
 

Air

 

Clean dry & oil free, 4.0 to 6.0 bar (58-87psi) with 75 Ltrs (2.6cu.ft) per minute flow

 
 
 
 
 

Exhaust

 

3m (10ft) exhaust pipe is provided which should be terminated outside building

 
 
 
 
 

Drain

 

3m (10ft) drain pipe provided which should be terminated into floor level drain

 
 
 
 
 

Operating environment conditions

 

+5 to +30°C (+41 to 86°F), 85% max RH (non condensing) ambient

 
 
 
 
 

 

 

 

 

 